MEMSnet Home: MEMS-Talk: RIE Etching Cr with PMMA Mask
RIE Etching Cr with PMMA Mask
2012-04-25
Judith Linacero
2013-01-12
冯跃
RIE Etching Cr with PMMA Mask
Judith Linacero
2012-04-25
Hi all,

I am looking for some RIE process to etch 50nm of Cr (e-beam evaporation
process) with 300nm of PMMA as a mask (after an E-Beam lithography with
patterns with 200nm of resolution).
I'm trying the process:
40 sccm Cl2+2sccm O2 with 200mT and 50W, but the etch rate of Cr is
about 8nm/min.
Do you know some different process to increase the etch rate and the
selectivity?

Best regards,
--

*JUDITH NOEMÍ LINACERO BLANCO*

*Plataforma de Nanotecnologia*

Parc Científic de Barcelona

c/ Baldiri Reixac 10-12

08028 Barcelona, Spain

*Tel.*       +34 934037138

*Fax.*      +34 934037109

[email protected] 

http://www.pcb.ub.es/plataforma/nanotecnologia

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Harrick Plasma, Inc.
Nano-Master, Inc.