Smooth DRIE made Si Mold for Hot Embossing
2012-05-29
XiXi
Smooth DRIE made Si Mold for Hot Embossing
XiXi
2012-05-29
Dear All,
I'm trying to use DRIE made silicon mold for hot-embossing.  I think there
are two potential problems:
1. Straight or undercut sidewall will make de-molding process in hot-emboss
difficult. I need to get 1 to 2 degree tapered side wall. Any good receipt
for Bosch process developed in Alcatel AMS 100?
2. *Scalloped* sidewall from Bosch process may prevent the plastic parts
de-molded from silicon mold. It seems a TMAH etching will smooth the
surface. Anyone has receipt or anyone can access this paper?
http://adsabs.harvard.edu/abs/2007IJTSM.127..187P
Many Thanks!
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.
MEMStaff Inc.