Can anyone provide me with some information about a wax that is compatible with
KOH etching. I am interested in waxing down a device silicon wafer to a surface
(such as glass) to protect the device side while the back side is exposed to
KOH for an extended period of time.

Thanks,
Dr. Kevin M. Walsh
Electrical Engineering Department, Speed Scientific School
University of Louisville, Louisville, KY 40292
(502) 852-0826
Internet address: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
University Wafer