SU-8 2025 spinning & crater formation
Tom Yuzvinsky
2012-11-10
Hi all,

I am spinning SU-8 2025 onto 4" silicon wafers and I have two possibly
related problems:

1. Unless I pour SU-8 to cover essentially the entire wafer, there is
a visible thickness transition between the region it was poured onto
and the region it was dispersed onto by spinning.
2. Soft baking the wafers on a hotplate creates millimeter wide
craters in the SU-8 layer.  They don't extend all the way to the wafer
but there is an obvious, large thickness variation.  A few craters
sometimes form during the 65C bake but many form during the 95C bake.
Prior to the bake the SU-8 looks nice, no bubbles.

I'm using Microchem's recommended process parameters.  I've tried
nanostripping the wafers beforehand, ashing them, letting the SU-8 sit
overnight before baking, nothing seems to help.  Any help or ideas
would be most appreciated!

Thanks,
Tom
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering