Adhesive to bond onto a carrier wafer for etching
2012-12-05
Shree Narayanan
2012-12-05
Tinka Li
2012-12-06
Michael Martin
2012-12-12
Shree Narayanan
2012-12-12
Michael Martin
2012-12-06
Felix Lu
2012-12-12
Shree Narayanan
2012-12-12
Bill Moffat
2012-12-12
Felix Lu
2012-12-06
Morrison, Richard H., Jr.
2012-12-12
Shree Narayanan
2012-12-12
MCNIE Mark
2012-12-07
basar bolukbas
2012-12-07
Shree Narayanan
2012-12-10
basar bolukbas
2012-12-12
Shree Narayanan
2012-12-07
Brian Stahl
2012-12-12
Shree Narayanan
2012-12-12
Brian Stahl
2012-12-11
Fei Wang
2012-12-12
Shree Narayanan
2012-12-12
Wangfei
2012-12-12
sangeeth kallatt
2012-12-07
Tang Tian
2012-12-12
Dave Roberts
2012-12-13
Xiaoguang Liu
Adhesive to bond onto a carrier wafer for etching
Tinka Li
2012-12-05
Hi Shree,

You meant something like Fomblin oil? 1 or 2 drops on your carrier,
smear out nicely, would do the chucking perfectly. Can also easily
remove (slide) your wafer out of your carrier wafer after DRIE. BUT, you
may have a little trouble in cleaning our wafer afterwards.

Prime Wafers
Rotterdam, NL

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Shree Narayanan
Sent: Wednesday, December 05, 2012 4:36 PM
To: General MEMS discussion
Subject: [mems-talk] Adhesive to bond onto a carrier wafer for etching

Hello all,

I need to mount a 4" silicon wafer on a 6" metallized carrier wafer, in
order to etch it in a Alcatel deep-reactive ion etcher. I am wondering
if
someone has used thermal vacuum grease for this purpose that can be
removed
easily at the end. The silicon wafer is patterned with photoresist and
has
no other material on it.

Thanks
Shree
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics