Gareth Jenkins
2012-12-04
Tinka Li
2012-12-05
Tinka Li
2012-12-05
Fahd Ali
2012-12-05
Tinka Li
etched glass
Gareth Jenkins
2012-12-06
I used only chrome with some oxide layer (just a low reflectivity chrome
mask blank) precoated with 0.5um AZ resist.
This was the cheapest and quickest option which is probably fine for most
purposes but some de-lamination and poor quality at the channel edge is the
downside. Cr/Au with a nice thick hard-baked resist is probably the best
method for high quality channels.


On 6 December 2012 14:49, Kuijpers, Peter wrote:

> Goodmorning,
>
> I was wondering what kind of mask was used to etch the glass in HF?
> Is het Cr or Cr/Au?
>
> best regards,
>
> Peter Kuijpers
> Senior Process Integrator
> Philips Innovation Services
> MiPlaza/TL group
> High Tech Campus 04-p4.20
> 5656 AE Eindhoven
> The Netherlands
> Phone: +31 402798904
> Mobile:+31 612507027,
> Email: [email protected]
>
> www.innovationservices.philips.com
>
>
> -----Original Message-----
> From: [email protected] [mailto:
> [email protected]] On Behalf Of
> Fahd Ali
> Sent: Wednesday 5 December 2012 16:41
> To: [email protected]
> Subject: Re: [mems-talk] etched glass
>
>
>
> Hi Nadim,
> I used HF to achieve high depth of the channels 200µm. does buffered oxide
> etchant can also give same result ?
>
> regards,Fahad
>
>
>
>
> > Date: Tue, 4 Dec 2012 18:16:34 -0300
> > From: [email protected]
> > To: [email protected]
> > Subject: Re: [mems-talk] etched glass
> >
> > Dear Fahad. Pure HF is very agressive to glass. You should use a
> > buffered oxide etchant based in ammonium fluoride. There are plenty of
> > recipes out there. Give it a try...
> >
> > Best regards
> >
> > Nadim
> > El 04/12/2012 20:48, "Fahd Ali"  escribió:
> >
> > >
> > > Hi,
> > >
> > > I have problem regarding glass etching. I made micro-channels using
> > > HF-40% on glass wafers. The problem is I have very sharp edges,
> > > which is not surprising. But for my application I need smooth edges.
> > >
> > > Is there any way during etching or after ?
> > > your answers are highly appreciated.
> > >
> > > regards,
> > > Fahad
> > > _______________________________________________
> > > Hosted by the MEMS and Nanotechnology Exchange, the country's
> > > leading provider of MEMS and Nanotechnology design and fabrication
> services.
> > > Visit us at http://www.mems-exchange.org
> > >
> > > Want to advertise to this community?  See http://www.memsnet.org
> > >
> > > To unsubscribe:
> > > http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > >
> > _______________________________________________
> > Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> > provider of MEMS and Nanotechnology design and fabrication services.
> > Visit us at http://www.mems-exchange.org
> >
> > Want to advertise to this community?  See http://www.memsnet.org
> >
> > To unsubscribe:
> > http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
> ________________________________
> The information contained in this message may be confidential and legally
> protected under applicable law. The message is intended solely for the
> addressee(s). If you are not the intended recipient, you are hereby
> notified that any use, forwarding, dissemination, or reproduction of this
> message is strictly prohibited and may be unlawful. If you are not the
> intended recipient, please contact the sender by return e-mail and destroy
> all copies of the original message.
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation