Adhesive to bond onto a carrier wafer for etching
2012-12-05
Shree Narayanan
2012-12-05
Tinka Li
2012-12-06
Michael Martin
2012-12-12
Shree Narayanan
2012-12-12
Michael Martin
2012-12-06
Felix Lu
2012-12-12
Shree Narayanan
2012-12-12
Bill Moffat
2012-12-12
Felix Lu
2012-12-06
Morrison, Richard H., Jr.
2012-12-12
Shree Narayanan
2012-12-12
MCNIE Mark
2012-12-07
basar bolukbas
2012-12-07
Shree Narayanan
2012-12-10
basar bolukbas
2012-12-12
Shree Narayanan
2012-12-07
Brian Stahl
2012-12-12
Shree Narayanan
2012-12-12
Brian Stahl
2012-12-11
Fei Wang
2012-12-12
Shree Narayanan
2012-12-12
Wangfei
2012-12-12
sangeeth kallatt
2012-12-07
Tang Tian
2012-12-12
Dave Roberts
2012-12-13
Xiaoguang Liu
Adhesive to bond onto a carrier wafer for etching
Shree Narayanan
2012-12-07
Dear Mr. Bolukbas,

Appreciate your response. Can you point me to a thermal band that you have
used. I googled up the term and couldnt come up with anything intelligent.
I have heard about this kind of tape form Nitto-Denko but I am wondering if
you are aware of a more easily sourced tape.

Thanks
Shree



On Fri, Dec 7, 2012 at 1:38 AM, basar bolukbas wrote:

>
> Dear Shree
>
> You can also try thermal band. It has got two similar side with a adhesion
> future. First you put it on your carrier. Then you remove protective
> coating on front side, so now you can put/stick your wafer on it. It has
> got very good thermal conductivity. As it will be smaller than your wafer,
> it will not react with your plasma, and you will not have a micromasking or
> contamination problem. After your etching process, put your carrier with
> your wafer on a hotplate @ 80C for a minute. Than you can easily remove
> your wafer from carrier. No residues no cleaning problems. :)
>
> Regards.
>
> > From: [email protected]
> > Date: Wed, 5 Dec 2012 10:36:21 -0500
> > To: [email protected]
> > Subject: [mems-talk] Adhesive to bond onto a carrier wafer for etching
> >
> > Hello all,
> >
> > I need to mount a 4" silicon wafer on a 6" metallized carrier wafer, in
> > order to etch it in a Alcatel deep-reactive ion etcher. I am wondering if
> > someone has used thermal vacuum grease for this purpose that can be
> removed
> > easily at the end. The silicon wafer is patterned with photoresist and
> has
> > no other material on it.
> >
> > Thanks
> > Shree
> > _______________________________________________
> > Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> > provider of MEMS and Nanotechnology design and fabrication services.
> > Visit us at http://www.mems-exchange.org
> >
> > Want to advertise to this community?  See http://www.memsnet.org
> >
> > To unsubscribe:
> > http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Harrick Plasma, Inc.