MEMSnet Home: MEMS-Talk: Spin-coating of thick photoresist over existing features
Spin-coating of thick photoresist over existing features
2012-12-20
João Tiago dos Santos Fernandes
2012-12-20
Gary Hillman
2012-12-20
Felix Lu
2012-12-21
Gareth Jenkins
2012-12-21
Lukasz Urbanski
2012-12-26
João Tiago dos Santos Fernandes
2012-12-26
Black, Robert
Spin-coating of thick photoresist over existing features
Gareth Jenkins
2012-12-21
Perhaps try covering the wafer in the resist solvent before pouring the
resist? This may help fill the gaps.

On 21 December 2012 02:57, João Tiago dos Santos Fernandes <
[email protected]> wrote:

> Hi everyone,
>
> I'm currently using AZ 40XT thick photoresist to make a 20-30 µm thin film
> over a Si sample with ~30 µm high SU-8 features.
>
> The problem I am facing is the following: when I pour the AZ on top of the
> sample, tiny air-bubbles are created in areas where SU-8 features are small
> (small wells, gaps, etc) - I'm guessing that this happens because the AZ is
> very viscous and isn't able to fill those spaces and traps air. When I spin
> coat, those tiny air bubbles are spread across the sample, compromising the
> process.
>
> Is there any way to get the air bubbles out of the way without
> compromising the final film thickness? I tried low rpm for a couple of
> minutes, with no success.
>
> Thank you so much,
>
> -----------------------------
> João Tiago dos Santos Fernandes
>
> INESC Microsistemas e Nanotecnologias (INESC MN)
> Rua Alves Redol, 9
> 1000-029 Lisboa
> Portugal
>
> Tel: +351 213100237
> Email: [email protected]
> URL: www.inesc-mn.pt
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing