Rajiv
2012-12-26
Dear all,
      I am using SU 8 (2150) for thickness of 800um coated on Si wafer. But for
me problems are,

(1) air bubble formation during soft baking process.
(2)wavy surface when hight increases.
(3) regarding SU -8 development, it takes time in hours.
I hope there will be solution.

Thanking you.

Regards,
Rajiv Panigrahi
Research scholar
CeNSE, IISc Bangalore

Sent from my Xperia™ smartphone smartphone

-------- Original Message --------
Subject: [mems-talk] Spin-coating of thick photoresist over existing features
From: João Tiago dos Santos Fernandes 
To: "[email protected]" 
CC:

Hi everyone,

I'm currently using AZ 40XT thick photoresist to make a 20-30 µm thin film over
a Si sample with ~30 µm high SU-8 features.

The problem I am facing is the following: when I pour the AZ on top of the
sample, tiny air-bubbles are created in areas where SU-8 features are small
(small wells, gaps, etc) - I'm guessing that this happens because the AZ is very
viscous and isn't able to fill those spaces and traps air. When I spin coat,
those tiny air bubbles are spread across the sample, compromising the process.

Is there any way to get the air bubbles out of the way without compromising the
final film thickness? I tried low rpm for a couple of minutes, with no success.

Thank you so much,

-----------------------------
João Tiago dos Santos Fernandes

INESC Microsistemas e Nanotecnologias (INESC MN)
Rua Alves Redol, 9
1000-029 Lisboa
Portugal

Tel: +351 213100237
Email: [email protected]
URL: www.inesc-mn.pt

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer