A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Double layer SU-8 fabrication problem
Double layer SU-8 fabrication problem
2013-01-12
Bill Chow
2013-01-13
Gareth Jenkins
2013-01-14
Bill Chow
2013-01-15
Gareth Jenkins
2013-01-15
Daniel Figura
2013-01-16
Jocelyn Ng
2013-01-16
Bill Moffat
2013-01-15
Black, Robert
2013-01-17
Gareth Jenkins
2013-01-23
Tinka Li
2013-01-23
Bill Chow
Double layer SU-8 fabrication problem
Daniel Figura
2013-01-15
Hello Bill,

I have recently done similar process (4 um + 20 um) and if I compare the
parameters I notice following differences:

> First layer 5um:
> Spin 3" Si wafer with SU-8 2002 at 500rpm for 5s, then 1000rpm for 30s.
        (similar)
> Softbake the sample  :1min@65C then 3 min@95C (hotplate)
        (I baked my 4 um layer for 1 + 4 min, so 5 um layer I would bake 1 +
5-6 min at 95)
> Expose it without waiting for 25s with a total of 125mJ/cm^-2
        (similar - I needed 200 mJ/cm2 on transparent substrate to get best
resolution so 125 mJ/cm2 on silicon sounds very real to me)
> Postbake it  without waiting for 1min@65C and 1min@95C (hotplate)
        (I would bake it much longer, 1 + 5-6 min. I bake my 4 um layer
1min/65C + 4 min 95C)


> Second layer 15um:
> Spin the second layer without waiting with SU-8 2010 at 500rpm for 5s,
> then 2000rpm for 30s.
> Softbake the sample 2min@65C then 5min@95C (hotplate)
        (I would bake 15 um layer at least 10 min at 95, I baked 20 um layer
12-15 min)
> Expose it without waiting for 45s with a total of 225mJ/cm^-2
        (Is there any need to increase the exposure dose? There is not much
light absorbed in 15 um layer of SU-8)
> Postbake it without waiting for 1min@65C and 2mailto:2min@95C (hotplate)
        (I again baked my layers much longer - same as SB)

My process was not optimized but worked fine for the goal and resolution we
needed.

Just to be sure - do you use open lid spin coater and contact exposure with
not-contaminated mask?


With best regards,

Daniel



Daniel Figura

smartfabgroupT Company

process consulting . data processing . fab software

Phone: +421 944 45 26 86

E-mail: [email protected], Web: www.smartfabgroup.com



Disclaimer notice: The information contained in this message and any
attachments is intended only for the personal and confidential use of the
designated recipient(s) named above. If you are not the intended recipient
of this message you are hereby notified that any review, disseminitation,
distribution or copying of this message is strictly prohibited. If you have
received this message by error, please notify the sender immediately.




-----Original Message-----
From: [email protected]
[mailto:[email protected]] On
Behalf Of Bill Chow
Sent: Sunday, January 13, 2013 16:21
To: General MEMS discussion
Subject: Re: [mems-talk] Double layer SU-8 fabrication problem

Thanks for your suggestion. I will try it tomorrow.

But the wrinkles exist in between the top and bottom layer. Also, It occurs
when I soft bake the second layer. That is before the exposure of the second

layer. I doubt why it happens at that time, but not when I soft bake the
first layer?

Bill

-----????-----
From: Gareth Jenkins
Sent: Sunday, January 13, 2013 1:50 PM
To: General MEMS discussion
Subject: Re: [mems-talk] Double layer SU-8 fabrication problem

By "dry skin" effect, I assume you mean wrinkles. Since they only occur in
the exposed area, this indicates insufficient crosslinking of the exposed
resist.
Either the post-exposure bake is not enough or your exposure dose is
insufficient (probably the exposure dose is the issue in my experience).
As for expiry date - 1 month is nothing. As long as it is stored OK it
should last well beyond the stated date.


On 12 January 2013 22:36, Bill Chow  wrote:

> Hi,
>
> I am working on a double layer structure with bottom layer 5um and top
> layer at 15um. I have used SU-8 2002 and SU-8 2010, however they have
> passed the expiry date for about a month (Would it be a problem?). In the
> last month, I was successed to make a beautiful sample out without any
> problem. However, Last week I tried to fabricate one more sample (due to
> misalignment of the structure in the first sample). I found there is a
> terrible problem arise. After I fabricated the first layer and spinned the
> 2nd layer, I put the sample on the 65C hot plate for soft bake. However,
> the sample shows a "dry skin" like structure between the interface of
> the
> first and second layer of SU-8 just after a few seconds on the hotplate. I
> don't know why a previously worked process could failed after a few
> weeks.... I have try to use the same bottle of SU-8 2010 and let the
> sample
> to cool down to room temperature before the second layer softbake, however
> the problem remains. A very interest point is that, only the exposed area
> have the "dry skin" appearance, for the unexposed area it don't have
> any
> problem. I hope someone could help me in this tough situation. Thanks.
>
> First layer 5um:
> Spin 3" Si wafer with SU-8 2002 at 500rpm for 5s, then 1000rpm for 30s.
> Softbake the sample  mailto:1min@65C then 3 min@95C (hotplate)
> Expose it without waiting for 25s with a total of 125mJ/cm^-2
> Postbake it  without waiting for 1min@65C and 1min@95C (hotplate)
>
> Second layer 15um:
> Spin the second layer without waiting with SU-8 2010 at 500rpm for 5s,
> then 2000rpm for 30s.
> Softbake the sample 2min@65C then 5min@95C (hotplate)
> Expose it without waiting for 45s with a total of 225mJ/cm^-2
> Postbake it without waiting for 1min@65C and 2mailto:2min@95C (hotplate)
>
> Regards,
> Bill
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing