MEMSnet Home: MEMS-Talk: SU-8 2005 overexposed?
SU-8 2005 overexposed?
2013-01-17
Jocelyn Ng
2013-01-18
Andrew Sarangan
2013-01-18
Gareth Jenkins
2013-01-19
Jocelyn Ng
2013-01-19
Gareth Jenkins
2013-01-21
Brubaker Chad
2013-01-21
Jocelyn Ng
2013-01-22
Brubaker Chad
2013-02-04
Jocelyn Ng
2013-02-04
Bill Moffat
SU-8 2005 overexposed?
Andrew Sarangan
2013-01-18
One possibility could be due to underexposure. The darkened edges could be
due to the sidewall slope, which is more pronounced at lower doses, and may
appear dark due to the light reflecting off the normal. At higher dose the
sidewall angles should start to straighten out.



On Wed, Jan 16, 2013 at 10:11 PM, Jocelyn Ng  wrote:

> Hello,
>
> I'm doing single layer SU8 2005, thickness ~6-7um. I use 60mJ/cm^-2 on
> sputtered gold surface. But somehow sometimes I notice that the edges of my
> pattern darkens, I suspect it's due to overexposed. But 60mJ is quite a low
> dose compared to the recommended one. I would appreciate any comments
> given. Thank you.
>
> Best Regards,
> Jocelyn
>
> Sent from my iPhone
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
The Branford Group