Emre Olceroglu
2013-01-30
Brian Stahl
2013-01-31
[email protected]
Dicing silicon with diamond blade
[email protected]
2013-01-31
Hi
you can do this. use 35KRPM. you will not get a nice cut because of the large
diamond particle size required to cut Pyrex.
if you need a better cut with less chipping, you will have to use a nickel blade
with less than 10u diamond. the nickel blade is also better because the resin
blades sometimes get rounded at the corners and as you use it more and more you
will not gwet a straight cut unless you go very deep into the support tape.
Shay

----- Original Message -----
From: Emre Olceroglu 
Date: Wednesday, January 30, 2013 21:23
Subject: [mems-talk] Dicing silicon with diamond blade
To: [email protected]

> Hello,
>
> I was wondering if I can dice 0.5mm silicon wafers with diamond
> blades that we normally use for Pyrex dicing.
>
> I know people dice bonded Silicon-Pyrex but I am not sure which
> blade they use.
>
> Thanks.
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
‭‮
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Nano-Master, Inc.