SU8 for Au Plating
Jocelyn Ng
2013-03-19
Dear all,

I'm using SU-8 2005.
I soft bake at 65C_540S, exposure dose is 60mJ and post exposure bake at
95C-120S.

Recently I encounter a problem where, after undergone gold plating process,
photoresist residue remains.
My stripping(remover PG) process is at 65C for an hour followed by acetone
bath in ultrasonic.
My plating temperature is about 45C for 25minutes.

I tried to strip in remover PG for another 30minutes but nothing seemed to
be working.
I had tried using the same condition previously and did not encounter this
problem.

I need some advice or comments on this.
Thanks a lot in advance.

Best Regards,
Jocelyn
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation