Hello everyone,

I'm trying to stick my polystyrene channel to glass, I tried some
methods likes hot bonding but it didn't work as I suffered the leaking,
does anybody has good suggestions?

Thanks a lot

--
Tong Chen
Postdoc
SyntheCell Team
IGDR CNRS UMR 6290
2, Avenue du Professeur Léon Bernard
35043 Rennes
France

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering