A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Silicon Nitride shorting metal layers
Silicon Nitride shorting metal layers
2013-04-29
nahid vahabi
2013-04-30
Michael Martin
2013-04-30
basar bolukbas
2013-04-30
Ruiz, Dan (SGNCOE)
2013-04-30
nahid vahabi
2013-04-30
Me
2013-04-30
[email protected]
Silicon Nitride shorting metal layers
[email protected]
2013-04-30
Hi Nahid


Can you please let me know what recipe you are using for silicon nitride. I
have worked on the same fab process PECVD nitride as dielectric layer on
gold. May be I will be able to help you.


Kind Regards

Hamood

----------------------------------------

From: "nahid vahabi" 

Sent: Tuesday, April 30, 2013 6:37 AM

To: "[email protected]" 

Subject: [mems-talk] Silicon Nitride shorting metal layers


Hello all,

I deposit a 250 nm PECVD SiN layer as the dielectric between two gold
layers and the metal layers seem to be short through the nitride each time.
I increased the nitride thickness to 400 nm and still the same. I gathered
that PECVD nitride is quite notorious for the pinholes so I multi-layered
the nitride (6 times of 40 nm each) to get rid of pinholes. It worked only
on 1 wafer and then the same problem again. So I appreciate any comments on
this and whether you think changing the dielectric is a good option.


Thank you,

Nahid

_______________________________________________

Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk



_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics