MEMSnet Home: MEMS-Talk: Process parameter for SU-8
Process parameter for SU-8
2013-05-01
Bill Chow
Process parameter for SU-8
Bill Chow
2013-05-01
Dear all,

I am working with Gersteltec’s GM1050 and GM1070. However, I found that the
process parameters suggested by the manual is not consistent, e.g. the exposure
time is similar for 3 – 8 um, prebake time is very long for 15um thick resist
(35min @ 95 degree). Do anyone has tested these parameters? I am frustated when
I am working with the manual. Should I just followed the Microchem manual
instead? Of course the spin coating process with be different, but PEB, softbake
ane exposure should be similar. Thanks.


Regards,

Bill Chow
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group