Remove aluminum mask after DRIE
HJ Rhee
2013-05-06
I'm trying to remove the aluminum layer (5000A, sputtered) that was used as
a hard mask for DRIE for structure release and having difficulty removing
it completely using the Al etchant (Al-12S).  There are residues left on
the surface (SiO2) that look like small grains, even after leaving the
wafer on the ethant (more than 1 hr). After a short-dip on BOE (~30s) and
putting in the etchant, the residues are reduced but still not completely
clean.

Anyone has an idea to completely remove these residues or has the same
experience? I don't quite understand why BOE helepd since shouldn't
aluminum oxide be only on the surface, not throughout the Al thin-film?

Thanks!!!
-Jenn
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.