MEMSnet Home: MEMS-Talk: high viscosity material
high viscosity material
2013-05-22
Xiao
2013-05-23
Andrew Sarangan
2013-05-23
Black, Robert
2013-05-24
Xiao
2013-05-24
조명래
high viscosity material
Black, Robert
2013-05-23
There are developable BARCs out there, but they only coat about 60nm. You may
have to double coat them. They are removed with developer.

-----Original Message-----
From: [email protected] [mailto:mems-talk-
[email protected]] On Behalf Of Xiao
Sent: Wednesday, May 22, 2013 3:14 AM
To: [email protected]
Subject: [mems-talk] high viscosity material

Hello everyone,

I am trying to find a high viscosity material that can fill pores (<100nm) of a
substrate, then do patterning with photoresist on it, and removed this material
with some solvent or even DI water, but not affecting the photoresist patterns.

We have tried several materials for now, but didn't work very well, do you have
any ideas of this material? Thank you!

Best regards,
Xiao
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
The Branford Group
MEMS Technology Review