Hello everybody,

we want to do hot embossing with PFA and Polystyrene, do you know where
we can buy nice and pure PFA and Polystyrene raw materials like pellets.

Thanks

--
Tong Chen
Postdoc
SyntheCell Team
IGDR CNRS UMR 6290
2, Avenue du Professeur Léon Bernard
35043 Rennes
France

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group
MEMS Technology Review