Hi Michael,
I can plate AuSn alloy on 2 inch - 200mm diameter wafer substrates.
I normally target on the Sn rich side of the eutectic (23% Sn) to make
certain low melting point.

Please give me a call to discuss the details.

Best regards,
Dave

David Roberts (Principal)
Silicon Valley Wafer Plating
807 Aldo Ave. Ste. 107 Santa Clara, CA 95054
(408) 469-3203
www.waferplating.com

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
The Branford Group