Hello all,

I'm doing hot embossing with epoxy and plastic, my structures are
10-40um large and 15-100um deep. I have some problems of sticking, when
I remove plastics from epoxy mold , it stuck a little and the structure
broke some time, does anybody had this problem and have solutions to
have nice small structure after remove from the epoxy mold.

Thanks very much

--
Tong Chen
Postdoc
SyntheCell Team
IGDR CNRS UMR 6290
2, Avenue du Professeur Léon Bernard
35043 Rennes
France

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
University Wafer
MEMStaff Inc.