2013-08-26
Hi Michael,     Your problem might be the exposure dose.  If you are using the
same time for glass and silicon for exposure, you might be under exposing the
photoresist because of the reflectivity difference in the two substrates.  This
might make the photoresist dissolve more slowly and, thereby, reduce the
apparent undercut rate for the LOR.
-Lou

> From: [email protected]
> To: [email protected]
> Date: Mon, 26 Aug 2013 16:32:40 +0000
> Subject: [mems-talk] LOR 3A and Borosilicate
>
> Hi,
>   Does anyone have experience with LOR3A (w/ 1827) on borosilicate glass.  The
processing parameters, i.e. undercut rate after a 6 min 150C bake, appear quite
different than those for silicon.  That is, I am seeing a much lower undercut
rate for the borosilicate than for silicon.
>
> Thank you,
>   Michael
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
MEMStaff Inc.
Tanner EDA by Mentor Graphics