Mask patterns for lithography resolution
SHANE GUO
2013-10-15
Hi all,
I am working with SU-8 molds for making microfluidic devices through
softlithography process. I am supposed to test our fabrication capability,
lithography resolution and spin coating uniformity. I need to design a mask
including features that can help me to find out the above things.
Do you guys know where I can find such mask patterns or references for designing
such patterns?
Thank you in advance for your help.
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review
Mentor Graphics Corporation