Gianmario Scotti
2013-11-04
조명래
2013-11-04
Gianmario Scotti
2013-11-05
Ricky Anthony
2013-11-05
MRC gmail
Etching of ALD titania (TiO2)
Gianmario Scotti
2013-11-01
Dear MEMS researchers,


do you know of a wet etchant that would remove ALD TiO2 from silicon? Some
of my colleagues told me that they don't know of anything suitable for ALD
films of TiO2 - only TiO2 nanoparticles. Incredulous, I hit google, but
came up with nothing - apparently, continuous films of TiO2 are quite a
challenge to etch with wet etchants.

Would any of you have a recipe that was tested as working with ALD TiO2?



Cheers!

--
Gianmario Scotti

Researcher
Aalto University, Dept. of Materials Science and Engineering
http://materials.aalto.fi/en/

Micronova, Tietotie 3
02150 Espoo
Finland
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group