MEMSnet Home: MEMS-Talk: Su8 2075 protocol for 300 um depth
Su8 2075 protocol for 300 um depth
2013-11-04
Sajeesh P
Su8 2075 protocol for 300 um depth
Sajeesh P
2013-11-04
Hi


I am in need of a fabrication of microchannel having a depth of 300 um. We
are doing soft lithography using PDMS. For that the silicon wafer we
prepared in Silicon. Su8 is used as the substrate. we have Su8- 2075 with
us.Sir can you share me the protocol for multilayer coating of su8- 2075
for getting a depth of 300 um over silicon wafer so that i can get a
channel of 300 um in PDMS during soft lithography.I searched a lot for this
multy layer coating for high AR channels.But i couldnt get anything.

Expecting your reply

Saj
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation