MEMSnet Home: MEMS-Talk: Anti-stiction coating
Anti-stiction coating
2013-12-03
Youmin Wang
2013-12-04
[email protected]
Anti-stiction coating
[email protected]
2013-12-04
hi,

if you have high electrical field on touchdown, you might be trapping charge in
the alumina and if not dissipated.

Shay

----- Original Message -----
From: Youmin Wang 
Date: Wednesday, December 4, 2013 2:49
Subject: [mems-talk] Anti-stiction coating
To: General MEMS discussion  PFDA
coated on ALD Alumina. But seems the stiction and adhesion are> still large. I
wonder if anyone of you have done surface treatment before the deposition of
PFDA on alumina? Thanks.

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review