MEMSnet Home: MEMS-Talk: Questions regarding HMDS (Hexamethyldisilazane)
Questions regarding HMDS (Hexamethyldisilazane)
2013-11-22
Sk Fahad Chowdhury
2013-12-16
Gianmario Scotti
2013-12-16
Bill Moffat
2013-12-16
Daniel Figura
2013-12-17
Andrew Sarangan
2013-12-17
Nathan McCorkle
FW: Questions regarding HMDS (Hexamethyldisilazane)
2013-12-17
Bill Moffat
Questions regarding HMDS (Hexamethyldisilazane)
2013-12-20
Nathan McCorkle
2013-12-20
Bill Moffat
Questions regarding HMDS (Hexamethyldisilazane)
Gianmario Scotti
2013-12-16
Hello Sk,


I am no HMDS expert, and am talking from memory, so don't take my word for
any of this:


1: Yes, I believe HMDS is polar, just by looking at the molecule.
2. and 3: HMDS forms a monolayer on SiO2, glass and hopefully (some)
metals, making the surface hydrophobic. Since we're talking of monolayers,
the thickness is probably below 1 nm. During sylilation by HMDS, some
ammonia may be produced.

You will find more info in this reference: F. Deyhimi, J. A. Coles, Helv.
Chim. Acta 65, 1752 (1982)
Rapid Silylation of a Glass Surface: Choice of Reagent and Effect of
Experimental Parameters on Hydrophobicity
http://onlinelibrary.wiley.com/doi/10.1002/hlca.19820650610/abstract







On Thu, Nov 21, 2013 at 8:17 PM, Sk Fahad Chowdhury <
[email protected]> wrote:

> Hi
>
> I have a few questions about hexamethyldisilazane or HMDS
> (CH3-Si-NH2-Si-CH3)
>
> 1.       1. Is HMDS a polar molecule? Is there any dipole present?
> electronegativity values of constituents are : H 2.2, C 2.55, Si 1.9, N
> 3.04. Carbon (2.55) - flourine (4) bonds are polar because of their
> electronegativity difference.
>
> 2.       2. How thick can HMDS on top of SiO2-Si be when it is dried in air
> from a liquid state? Can the thickness of HMDS be determined when it is air
> dried?
> 3. If HMDS is air dried and some molecules are left in sample, is it going
> to be HMDS molecule or it will be something else? Will it release ammonia?
> Also will it be a continuous layer or there will be clustering?
>
> Thanks a lot :)
>
> regards
>
> Sk
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>



--
Gianmario Scotti

Researcher
Aalto University, Dept. of Materials Science and Engineering
http://materials.aalto.fi/en/

Micronova, Tietotie 3
02150 Espoo
Finland
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing