A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Shipley 1827 resist without hmds or p20 primer
Shipley 1827 resist without hmds or p20 primer
2014-01-13
Haider, Ahmad M
2014-01-13
Robert Bock
2014-01-14
Andrew Sarangan
2014-01-14
Daniel Figura
2014-01-14
Bill Moffat
Shipley 1827 resist without hmds or p20 primer
Robert Bock
2014-01-13
Ahmad,

I have used Shipley 1805 for years and always got bad results if the primer
step wasn't done properly.  While it might work for your particular process,
without primer the process window is very small and I would suspect you'd
have under-etch and/or washout issues.

I'd run some experiments and see; if you do, do tell us the results!

Regards,
Robert Bock


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf
Of Haider, Ahmad M
Sent: Monday, January 13, 2014 12:17 PM
To: [email protected]
Subject: [mems-talk] Shipley 1827 resist without hmds or p20 primer

Hi,

I am using Shipley 1827 resist for photolithography. Till now, I always have
a pre step in which I spin p20 primer onto the wafer and then I spin the
1827 resist onto the wafer. I am facing certain problems with this. Can I
just spin 1827 on a clean wafer directly? Can I get some help with the
process parameters?

Thanks
Ahmad
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing