Haider, Ahmad M
2014-01-13
Robert Bock
2014-01-14
Andrew Sarangan
2014-01-14
Daniel Figura
2014-01-14
Bill Moffat
Shipley 1827 resist without hmds or p20 primer
Bill Moffat
2014-01-14
Ahmad, in 1969 IBM patented the use of HMDS as a primer.  By baking 200 wafers
at 150 degrees C then spinning on wet HMDS and spin drying.  Then applying
resist.  This was modified in 1980 by YES by vacuum dehydrating the substrate
and using the vacuum to create a vapor of HMDS.  Vacuum vapor prime was born and
has been used since then as the superior method of creating resist adhesion.  We
at YES have the ability to prime your wafers send them back and they will
survive weeks of outside atmosphere without hurting the adhesion.  Please
contact me for free tests.  Bill Moffat. 925 373 8353 or cell phone 408 590
4577.

-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of Haider,
Ahmad M
Sent: Monday, January 13, 2014 12:17 PM
To: [email protected]
Subject: [mems-talk] Shipley 1827 resist without hmds or p20 primer

Hi,

I am using Shipley 1827 resist for photolithography. Till now, I always have a
pre step in which I spin p20 primer onto the wafer and then I spin the 1827
resist onto the wafer. I am facing certain problems with this. Can I just spin
1827 on a clean wafer directly? Can I get some help with the process parameters?

Thanks
Ahmad
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing