A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: for forming center hole(radius 10~15um) on 2um thickness Ni membrane(radius 300um)
for forming center hole(radius 10~15um) on 2um thickness Ni membrane(radius 300um)
2014-01-24
김덕수
2014-01-24
王舒禹
2014-01-24
MRC gmail
for forming center hole(radius 10~15um) on 2um thickness Ni membrane(radius 300um)
王舒禹
2014-01-24
Second method. Lift off takes longer time.

On Friday, January 24, 2014, 김덕수  wrote:

> Hi.
>
> at first, I want you to understand that I don't know english very well.
>
>
> I want to form center holes on Ni membrane.
> 
> diameter of membrane is 3~400um(thickness 2um) and of center hole is
> 2~30um.
> 
> I want to form 5 center holes.
>
> So I thought two methods.
>
>
> 1. Using lift-off process, center holes is formed without etching process.
> 2. after deposition Ni thin film,  etching process is progressed for
> forming center holes.
>
>
> I want to know which is more efficient.
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Mentor Graphics Corporation