Antonino Miceli
2014-02-16
Bill Moffat
2014-02-16
Bill Moffat
Bonding LTG:GaAs to SiN?
Bill Moffat
2014-02-16
If you want to test plasma bonding I can help. Bill Moffat

Sent from my iPad

On Feb 16, 2014, at 6:27 AM, "Antonino Miceli"  wrote:

> Hi all,
>
> We are trying to bond LTG:GaAs to SiN. Does anyone have experience with
> this? Any references?
> Would an SiO2 adhesion layer help?
>
>
> We are trying to make a photoconductive switch on a SiN membrane (released
> after bonding!).
>
> Thanks,
> Nino
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics