A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Wet etching PDMS (KOH etch mask)
Wet etching PDMS (KOH etch mask)
2014-01-22
Abhinav Jain
2014-01-23
Andrew Sarangan
2014-01-23
Daniel Vercosa
2014-01-23
John Bohland
2014-02-26
Abhinav Jain
Wet etching PDMS (KOH etch mask)
Abhinav Jain
2014-02-26
Thanks all for your replies.
Based on different replies, I feel the that best solution is to use a solid
chuck with sealing rings to protect one side. Does anyone any company which
provides these type of chucks in US?

Thanks
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing