MEMSnet Home: MEMS-Talk: SU8 adhesion problems
SU8 adhesion problems
2014-03-10
Janis Klavins
2014-03-11
Nadim Morhell
2014-03-11
王舒禹
2014-03-11
Sophie Roman
2014-03-11
Bill Moffat
2014-03-11
Janis Klavins
2014-03-12
Parrish Ralston
2014-03-11
João Tiago dos Santos Fernandes
SU8 adhesion problems
Nadim Morhell
2014-03-11
I had similar problems when coating  thick layers of SU8 on soda lime
glass. Be careful when removing the substrate from the hotplate at 95
degrees as thermal shocks cracks the SU8 unbonding it from the glass.

The parameters that you use for soft bake sugests that you are coating a
thin layer of SU8.  ( Less than 10 microns).  I haven't got this problem
with thin layers.

Maybe You should check how long you leave it on the hotplate, I ussually
have it for longer times than those you posted.

You can also try more exposure time. It may spoil the patterns but you can
check if it works...

El 10/03/2014 20:40, "Janis Klavins"  escribió:

> Hello everybody,
>
> I am trying to coat an SU8 material on ITO etched glass. I have a problem
> that during development the SU8 lifts off the glass very easily. if the
> glass sheet is immersed in the developer the SU8 lifts off and floats away.
>
> I believe that this is a baking problem (too much or not enough) after
> coating the SU8. I am using a two step kiln 65 degrees ( 1 min)  and 95
> degrees (4 min). The same settings for post exposure bake.
>
> Has anyone seen a problem like this?
>
> --
> Best regards,
> Mr. Janis Klavins
> EuroLCDs
> Phone: +37163600300
> Mobile: +37126141049
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.