su-8 2002 removal method
2014-04-03
김덕수
2014-04-03
shay kaplan
2014-04-04
Tong CHEN
2014-04-04
Jerry Chen
2014-04-07
Amit Kumar
2014-04-08
bhargav panchal
su-8 2002 removal method
김덕수
2014-04-03
I used SU-8 2002 for sacrificial layer(about 2um).

after whole process is finished, I want to remove SU-8 layer.

but, it is very hard. I used Remover PG(80℃, 30min) but it is
indissolubleness(?).

For forming mems sensor, the metal layers are deposited around a SU-8 layer.

So I want to remove SU-8 2002 without damages of other structures.

How can I do it?
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
University Wafer
MEMS Technology Review