Protek B3 removal procedure
2014-04-23
Haider, Ahmad M
2014-05-07
Kagan Topalli
Protek B3 removal procedure
Haider, Ahmad M
2014-04-23
Hello,

Has anyone used Protek B3 coating for protection against KOH and knows how to
effectively REMOVE it after KOH etch? I am doing a process in which I am using
4.5 um of Protek B3 coating to protect my Silicon nitride cantilevers against
KOH etch. I would like to know how to REMOVE the B3 coating after the KOH etch?
Both dry and wet removal processes would be helpful.
Note: Since my underlying layer is silicon nitride, will using CF4/O2 mixture to
remove B3 coating, remove silicon nitride as well?

Thanks
Ahmad
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics