Substrate temperature in Ebeam
2014-05-05
Ashay Chitnis
2014-05-06
Ruiz, Dan (SGNCOE)
Substrate temperature in Ebeam
Ruiz, Dan (SGNCOE)
2014-05-06
Asc,

It really depends on your process, but we were able to use Ebeam evaporation for
lift-off metal.  Since the resist would reflow at about 120C, I can safely say
we were below that temperature.

If I remember right, the temperature gauges we used setting up the process said
we were reaching temperatures of about 100C regularly.

Dan

-----Original Message-----
From: [email protected] [mailto:mems-talk-
[email protected]] On Behalf Of Ashay Chitnis
Sent: Saturday, May 03, 2014 2:42 AM
To: [email protected]
Subject: [mems-talk] Substrate temperature in Ebeam

Hi,

I would like to know temperature of substrate in ebeam and sputter for standard
metals and dielectrics.

Asc
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.