MEMSnet Home: MEMS-Talk: Alignment problem with Multilayer SU-8 fabrication
Alignment problem with Multilayer SU-8 fabrication
2014-05-15
[email protected]
2014-05-14
Bill Chow
2014-05-14
Gareth Jenkins
2014-05-14
[email protected]
2014-05-16
Jiho Song
2014-05-16
Daniel Figura
2014-05-16
hamideh jafarpoor
2014-05-16
王舒禹
2014-05-16
Matthieu Nannini
2014-05-16
sangee vs
2014-05-19
[email protected]
Alignment problem with Multilayer SU-8 fabrication
Jiho Song
2014-05-16
Bill,

You can make the mask with the design that has the alignment mark on left
and right edge of wafer.

So, you can spin-coat the first layer and drop some developer on both left
and right edge of wafer, then you will able to see clearly where to align
the second layer. Of course, you need the exactly same align mark on your
second layer pattern.

Let me know if this is clear.

Thanks.
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group