Exposure with uncollimated light source
Daniel Figura
2014-08-05
Hello everybody,

A few weeks ago Dimitar  posed an interesting question about issues exposing
and SU8 with uncollimated lamp and that started me thinking about limits of
such approach. Few days later I was myself in theoretical discussion about
using uncollimated lamp as a light source for lithographic exposures. I
believe that the main limitation is geometrical light travel path; that you
basically expose parts of the substrate under severe angle which blurs your
image, but I might be wrong.

Does anyone of you is using uncollimated light source for contact/proximity
exposure? What is the configuration you use (size of lamp, distance, resist
thickness) and results do you achieve?

Thanks for the answers.

With best regards,

Daniel


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.
Harrick Plasma, Inc.