A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Coating problem of su8 10 over the silicon wafer
Coating problem of su8 10 over the silicon wafer
2014-08-25
Sajeesh P
2014-08-28
"João Tiago S. Fernandes"
Coating problem of su8 10 over the silicon wafer
Sajeesh P
2014-08-25
Hi

We are trying to coat su8 10 over the silicon wafer for a thickness of
resist 20 um. The protocol specified by Micro chem is followed for this
thickness.Spin speed of 1590 rpm with acceleration of 300 rpm and 30
seconds. The problem is, after coating the Su8 over the wafer, suddenly
resist form islands over the wafer (resist balling up and leaving small
empty pores). Thus the channels of 10 um is not possible to form.

We also tried to coat an HMDS coating to improve the adhesion. But the
balling up effect increased. Instead of small diameter pores, It form large
diameter vacant spaces.

We done an HF dip (1: 5 ratio) before the coating of su8 and dehydration of
wafer with 150 C at about 10 minutes.Is it problem of lack of cleaning of
wafer. Any other cleaning procedure should follow for this?

Please suggest me some remedy for this

--
Sajeesh P
Mechanical Engineering Dept
IIT Madras
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
University Wafer
Tanner EDA by Mentor Graphics