MEMSnet Home: MEMS-Talk: Electroplating Dielectric Material
Electroplating Dielectric Material
2014-09-15
Ricky Anthony
2014-09-16
Robert Bock
2014-09-16
André Bödecker
Electroplating Dielectric Material
André Bödecker
2014-09-16
Hello,

on some metals like (titanium, tantalum a. o.) it is possible to form an
insulating oxide layer by polarity reversal in special electrolytes (also
called anodizing).

Regards,
André

-----Ursprüngliche Nachricht-----
Von: [email protected]
[mailto:[email protected]] Im
Auftrag von Ricky Anthony
Gesendet: Sonntag, 14. September 2014 18:55
An: [email protected]
Betreff: [mems-talk] Electroplating Dielectric Material

Hi,

I was wondering if there is any dielectric (or poor semiconductor) which can
be electroplated on conductive surface like Nickel. Could you give brief
process for it?

Thanks,

Ricky Anthony

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation