MEMSnet Home: MEMS-Talk: Tips for fabrication of microchannel heat sinks
Tips for fabrication of microchannel heat sinks
2015-04-22
Leily Majidi
2015-04-23
Gianmario Scotti
2015-04-23
André Bödecker
2015-04-23
shay
Tips for fabrication of microchannel heat sinks
André Bödecker
2015-04-23
Hello Leily,

holes in the glass wafers is one of the best ways to connect the
microchannels. There are different techniques like drilling, ultrasonic
drilling, laser and powder blasting. For getting enough fluid through the
inlets they should have a width of several hundreds of µm. For doing powder
blasting you can contact me: [email protected]

Regards,
André Bödecker


-----Ursprüngliche Nachricht-----
Von: [email protected]
[mailto:[email protected]] Im
Auftrag von Leily Majidi
Gesendet: Mittwoch, 22. April 2015 00:21
An: [email protected]
Betreff: [mems-talk] Tips for fabrication of microchannel heat sinks

Hello,

For my project, I want to fabricate microchannels on silicon wafer and I
need some help.I have a 4 inch silicon wafer and my channels are going to be
etched on chips with the dimensions of 15 mm by 15 mm. The channels are
300 micron deep and the smallest width of channels is 50 microns. Another
thing is that my coolant is a segmented glow containing liquid metal
(Galinstan) and mineral oil, and Galinstan is corrosive to metals.
I read in different literature that anodic bonding is used to cover the chip
with glass. If I use the same process, how can I connect my inlet and outlet
tubes to the chip to pump the coolant? Should I make holes on glass?

I'd appreciate any help.
Thank you
Leily
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
The Branford Group
Mentor Graphics Corporation