Hi,

I am a graduate student, who has just started work on MEMS.
My work needs bonding glass anodically to both sides of
single-crystal silicon.We bonded glass to one side of the wafer and then
tried bonding glass to the other side as well.
But it does not work in spite of doubling the applied voltage.
Any suggestions/references about this will be most welcome.

Debjani

Research Scholar (Semiconductor Group)
Department of Physics                 Ph: (080)309-2316
Indian Institute of Science           Fax:(080)334-1683
Bangalore - 560012


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.