A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PDMS bonding to silicon for micro-channel heat sinks
PDMS bonding to silicon for micro-channel heat sinks
2015-06-09
Leily Majidi
2015-06-10
André Bödecker
2015-06-11
Nathan McCorkle
2015-06-15
André Bödecker
2015-06-16
Bill Moffat
PDMS bonding to silicon for micro-channel heat sinks
André Bödecker
2015-06-15
Hello Nathan,

dicing away the area of the edge bead is the only way.

Regards,
André

-----Ursprüngliche Nachricht-----
Von: [email protected] [mailto:mems-
[email protected]] Im Auftrag von Nathan
McCorkle
Gesendet: Mittwoch, 10. Juni 2015 20:29
An: General MEMS discussion
Betreff: Re: [mems-talk] PDMS bonding to silicon for micro-channel heat sinks

On Tue, Jun 9, 2015 at 10:37 PM, André Bödecker 
wrote:
> Hello Leily,
>
> anodic bonding is an expensive, but very reliable process. Structuring
> of glass wafers is not a big problem. You can contact me if you are
interested.
>
> Bonding with PDMS normally needs only an oxygen plasma activation of
> the surfaces. There are also some special adhesion promoters if
> necessary. But a tight bonding will only work if the PDMS has a good
> uniformity and that will be a difficulty over a whole 100 mm wafer, I
> assume. We use the Sylgard 184 2k-silicone ("PDMS"; Dow Corning). Even
> spin-coating leads to an edge bead which inhibits a complete contact between
two wafers.

How do you get around this? Do you adjust the spin-coating or viscosity of the
resin? Or do you simply cut/dice the bead area away?
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
The Branford Group
Tanner EDA by Mentor Graphics