Dear all,



for structuring gold layers I’m using Au etch 200 from NB technologies as a
standard process which has a very good performance. But now there is a
demand for a good selectivity to copper. It seems that there is no gold
etchant available with a selectivity to copper. Does somebody have any
suggestions?



Regards,

Mit freundlichem Gruß



André Bödecker



_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Addison Engineering
The Branford Group