MEMSnet Home: MEMS-Talk: Best way to make elemental Cr films
Best way to make elemental Cr films
2015-10-14
Ali Alsaqqa
2015-10-15
André Bödecker
2015-10-16
Andrew Sarangan
2015-10-19
Ali Alsaqqa
2015-10-20
Andrew Sarangan
2015-10-26
Ali Alsaqqa
2015-10-19
[email protected]
Best way to make elemental Cr films
[email protected]
2015-10-19
Anther thing to keep in mind is that the Cr will act as a getter within the
vacuum chamber.  So if you run the Cr deposition for a while with the shutter
closed you will essentially scavenge residual oxygen.

Regards,
  Michael
________________________________________
From: [email protected] [mems-talk-
[email protected]] on behalf of Andrew Sarangan
[[email protected]]
Sent: Friday, October 16, 2015 10:55 AM
To: General MEMS discussion
Subject: Re: [mems-talk] Best way to make elemental Cr films

The 10^-7 Torr during evaporation is a pretty decent vacuum level, and the
oxidation rate should be very minimal especially if you keep the deposition
rate high.



On Mon, Oct 12, 2015 at 8:44 PM, Ali Alsaqqa  wrote:

> Hello all,
>
> I would like to know what is the best way to prepare films of elemental
> Chromium. Exact thickness does not matter, but something like hundreds of
> nanometers should be fine. The target measurement is simple transport (I,
> V) in the presence of some magnetic field.
>
> My main concern here is oxidization. I was thinking about depositing the
> films using e-beam evaporator, but it can attain a vacuum of only 10-7
> Torr, and with this level oxidization will occur. MBE is not an option at
> the moment.
>
> I was also thinking about buying wafers from commercial sectors, but I will
> run into the same problem, i.e. the surface will oxidize as soon as it
> contacts air.
>
> Are there any suggestions?
>
> Ali M. Alsaqqa,
> PhD candidate,
> Department of Physics,
> University at Buffalo, NY, USA
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at https://urldefense.proofpoint.com/v2/url?u=http-3A__www.mems-
2Dexchange.org&d=AwICAg&c=SgMrq23dbjbGX6e0ZsSHgEZX6A4IAf1SO3AJ2bNrHlk&r
=iuM4gMLa1Lu9rB1E3CyO_FZKwp19zNE1F2fh6h-VHUI&m=C7vFsk2RBX_gPVOaDYVvx43aSypywMKVW
6z37Q3mEpk&s=S1eSboBUWlH_tqVJfoHjHcVj2fIOHHI7fQlnVKe3QeQ&e=
>
> Want to advertise to this community?  See
https://urldefense.proofpoint.com/v2/url?u=http-
3A__www.memsnet.org&d=AwICAg&c=SgMrq23dbjbGX6e0ZsSHgEZX6A4IAf1SO3AJ2bNrHlk&r
=iuM4gMLa1Lu9rB1E3CyO_FZKwp19zNE1F2fh6h-
VHUI&m=C7vFsk2RBX_gPVOaDYVvx43aSypywMKVW6z37Q3mEpk&s=wSQJ2I-
cIsJay6yeI5v0k83yM6LRDIL6A8QrA9Mdaq4&e=
>
> To unsubscribe:
> https://urldefense.proofpoint.com/v2/url?u=http-3A__mail.mems-2Dexchange
.org_mailman_listinfo_mems-
2Dtalk&d=AwICAg&c=SgMrq23dbjbGX6e0ZsSHgEZX6A4IAf1SO3AJ2bNrHlk&r
=iuM4gMLa1Lu9rB1E3CyO_FZKwp19zNE1F2fh6h-
VHUI&m=C7vFsk2RBX_gPVOaDYVvx43aSypywMKVW6z37Q3mEpk&s=XOcJTiaBHb48gWyBz-
E8jlHjKQVOdqOo7PVrOuMmjLI&e=
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at https://urldefense.proofpoint.com/v2/url?u=http-3A__www.mems-
2Dexchange.org&d=AwICAg&c=SgMrq23dbjbGX6e0ZsSHgEZX6A4IAf1SO3AJ2bNrHlk&r
=iuM4gMLa1Lu9rB1E3CyO_FZKwp19zNE1F2fh6h-VHUI&m=C7vFsk2RBX_gPVOaDYVvx43aSypywMKVW
6z37Q3mEpk&s=S1eSboBUWlH_tqVJfoHjHcVj2fIOHHI7fQlnVKe3QeQ&e=

Want to advertise to this community?  See
https://urldefense.proofpoint.com/v2/url?u=http-
3A__www.memsnet.org&d=AwICAg&c=SgMrq23dbjbGX6e0ZsSHgEZX6A4IAf1SO3AJ2bNrHlk&r
=iuM4gMLa1Lu9rB1E3CyO_FZKwp19zNE1F2fh6h-
VHUI&m=C7vFsk2RBX_gPVOaDYVvx43aSypywMKVW6z37Q3mEpk&s=wSQJ2I-
cIsJay6yeI5v0k83yM6LRDIL6A8QrA9Mdaq4&e=

To unsubscribe:
https://urldefense.proofpoint.com/v2/url?u=http-3A__mail.mems-2Dexchange
.org_mailman_listinfo_mems-
2Dtalk&d=AwICAg&c=SgMrq23dbjbGX6e0ZsSHgEZX6A4IAf1SO3AJ2bNrHlk&r
=iuM4gMLa1Lu9rB1E3CyO_FZKwp19zNE1F2fh6h-
VHUI&m=C7vFsk2RBX_gPVOaDYVvx43aSypywMKVW6z37Q3mEpk&s=XOcJTiaBHb48gWyBz-
E8jlHjKQVOdqOo7PVrOuMmjLI&e=
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
University Wafer