How to make a metal grid
2016-07-05
John Bohland
2016-07-06
Bill Moffat
2016-07-06
Bill Moffat
2016-07-06
Gary Hillman
2016-07-06
[email protected]
2016-07-07
Philipp Altpeter
2016-07-07
Wilson, Thomas
2016-07-07
Andrew Sarangan
2016-07-12
Daniel Figura
2016-07-12
Roberto Igal Chertkow
2016-07-13
John Bohland
How to make a metal grid
Daniel Figura
2016-07-12
Hello John,

How many substrates do you actually need?

Daniel

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On
Behalf Of John Bohland
Sent: Wednesday, June 29, 2016 2:57 AM
To: [email protected]
Subject: [mems-talk] How to make a metal grid

I am interested in making a metal grid on a 370 mm X 470 mm glass substrate.

The problem is that the metallization lines must be only 1.5 microns in
width and spaced (pitch) only a few microns apart.

The metal can be Al or Ag and 100 nm thick.

The best idea I have is to monolithically coat the glass with sputtered
(PVD) Al or Ag then use a picoseond laser to remove all but the desired 1.5
micron wide metal line widths. Even then I don't know if the laser would
have good enough resolution to meet these requirements.

Anyone have better ideas?

Thanks,

John

NOTICE
This transmittal and/or attachments ("Communication") is confidential to
Bloo Solar, or may otherwise be privileged information. If you are not the
intended recipient, you are hereby notified that you have received this
Communication in error and any dissemination, distribution or copying of
this Communication is strictly prohibited. If you have received this
Communication in error, please notify us immediately and promptly delete and
purge this Communication.

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.
MEMStaff Inc.