MEMSnet Home: MEMS-Talk: -|EXT|- Re: Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-19
Mehmet Yilmaz
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-19
Mehmet Yilmaz
2017-05-01
André Bödecker
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-04-20
Sangwook Chu
2017-05-01
Orozaliev Ajymurat Nurdinovich
Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-05-01
mercado
2017-05-03
April Maria Lujan
-|EXT|- Re: Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
2017-05-04
MCNIE Mark
2017-05-05
Mehmet Yilmaz
-|EXT|- Re: Removal of dicing tape (DENKA T-80HW-23A) residues from silicon surface of MEMS chips
MCNIE Mark
2017-05-04
If you spin a layer of resist on before applying dicing tape that should help.

It is also possible to get custom dicing tape with cavities or no adhesive over
device areas.

Regards,

Mark

Mark McNie
Principal Applications Engineer
Oxford Instruments Plasma Technology

> On 4 May 2017, at 01:48, April Maria Lujan 
wrote:
>
> Hi Mehmet,
>
> IPA works well to remove adhesive redsidue, you should try that and finish
> with an 180 second O2 clean.
>
> There's 91% IPA that is sold at local drug stores and the 99% IPA which is
> used by industry which should work well.
>
> Other that acetone is not very great. Try IPA...
>
> Best regards,
>
> April Lujan
>
> Manufacturing Technician
>
>> On Fri, Apr 21, 2017 at 8:37 AM, mercado  wrote:
>>
>> Hi Mehmet,
>>
>> Yes, try with Piranha clean, serveral times if it's necessary.
>>
>> Best,
>>
>> Dante Mercado
>>
>> El 2017-04-20 01:10, Sangwook Chu escribió:
>>
>>> Hi Mehmet,
>>>
>>> Can you try Piranha clean? I am not sure what materials you have on your
>>> chip but it should work great for removing organic residues.
>>>
>>> Best,
>>> Sangwook
>>>
>>> On Wed, Apr 19, 2017 at 11:33 PM Mehmet Yilmaz 
>>> wrote:
>>>
>>> Dear mems-talk community,
>>>> I am using "DENKA T-80HW-23A" dicing saw tape to dice MEMS chips from
>>>> full
>>>> 4" silicon wafers.
>>>>
>>>> My integration process does not allow me to mechanically peel the diced
>>>> tape from the diced MEMS chips. So, I tried acetone to remove the dicing
>>>> saw tape (DENKA T-80HW-23A) pieces from the silicon surface of the MEMS
>>>> chips. The pieces of dicing tape are removed from the MEMS chips,
>>>> however,
>>>> I realized that, there are very thin layers of residues left on the
>>>> silicon
>>>> surface of the MEMS chips that I cannot remove with acetone.
>>>>
>>>> After drying the MEMS chips with nitrogen blowing, I tried O2 plasma
>>>> clean
>>>> to remove the remaining residues. Most of the residues are gone, but
>>>> there
>>>> are still some residues left that I need to remove.
>>>>
>>>> Could you please let me know how to remove these thin residues of the
>>>> dicing saw tape (DENKA T-80HW-23A) from silicon surface?
>>>>
>>>> Thanks in advance,
>>>> Sincerely,
>>>>
>>>> Mehmet
>>>> _______________________________________________
>>>> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
>>>> provider of MEMS and Nanotechnology design and fabrication services.
>>>> Visit us at http://www.mems-exchange.org
>>>>
>>>> Want to advertise to this community?  See http://www.memsnet.org
>>>>
>>>> To unsubscribe:
>>>> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>>>>
>>>> --
>>> Sangwook Chu
>>>
>>> Ph.D Student
>>> MEMS Sensors and Actuators Laboratory
>>> Department of Electrical and Computer Engineering
>>> University of Maryland
>>> College Park, MD, USA
>>> Tel: +1-301-405-1897
>>> Cel: +1-301-332-9260
>>> Email: [email protected] 
>>> _______________________________________________
>>> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
>>> provider of MEMS and Nanotechnology design and fabrication services.
>>> Visit us at http://www.mems-exchange.org
>>>
>>> Want to advertise to this community?  See http://www.memsnet.org
>>>
>>> To unsubscribe:
>>> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>>>
>> _______________________________________________
>> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
>> provider of MEMS and Nanotechnology design and fabrication services.
>> Visit us at http://www.mems-exchange.org
>>
>> Want to advertise to this community?  See http://www.memsnet.org
>>
>> To unsubscribe:
>> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
>
> +++Scanned for Viruses by ForcePoint+++


___________________________________________________________________________This
e-mail is confidential and is for the addressee only.  Please refer to
www.oxinst.com/email-statement for regulatory information.
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.
Nano-Master, Inc.