On the topic of critical point drying - CPD
2018-05-24
Thomas W Frisk
On the topic of critical point drying - CPD
Thomas W Frisk
2018-05-24
Dear Colleagues,

We are doing some CO2 critical point drying of silicon structures. Not getting a
very good yield, the question came up: what protocol do you use?

I did some googling, and found three distinctly different protocols (at least).

1. Multiple exchanges: 120 cycles totaling approx. 15 minutes

2. A number of exchanges: 5-10 cycles totaling approx.. 30 minutes

3. One-two exchanges: 1-2 cycles totaling approx. 1,5-2 hours

I guess it comes down to the question: what works better in your application?
"Series dilutions" or "molecular transport through diffusion"

I would happily read a few lines on your results and experiences ;-) on the
matter. It would be neat to get a better understanding of the scenarios where
this or that works better.

Best regards,

Thomas Frisk
Researcher,
Biomedical and X-Ray Physics,
Dept. of Applied Physics,
KTH, Stockholm, Sweden

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Nano-Master, Inc.
Mentor Graphics Corporation