Hello,

i intend to do contact lithography on a BCB-film (a polymer film) which is
spun on a rectangular glass sample. For the given application i need
resolution which is as high as possible. Unfortunately the resolution is
still unsatifactory. I believe that it is caused by the edge bead of the
BCB-film and the photoresist.
 I try to remove the photoresist edge bead by exposing and developing the
edge, using a simple shadow mask. That works fine when doing lithography on
glass only.
 I try to remove the bcb edge by etching it, using RIE. I can't measure any
remaining edge bead. Nevertheless the resolution on BCB films is much worse
than that on glass alone.

Thank you for any comments,

     Jan Sundermeyer
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
MEMStaff Inc.
University Wafer