MEMSnet Home: MEMS-Talk: RE:Thermal properties of SU8/Epoxy?
RE:Thermal properties of SU8/Epoxy?
1999-08-04
Paul Lethbridge
RE:Thermal properties of SU8/Epoxy?
Paul Lethbridge
1999-08-04
Here's the thermal conductivity for an epoxy mold used in BGA packaging
to get you started:

PLASKON-SMT-B1                  Thermal conductivity, Isotropic
KXX=KYY=KZZ=0.71 W/m*K

Here's Plaskon's link http://www.amocochem.com/PlaskonSite/smtb1.html
and another link with some other epoxy data
http://www.epoxies.com/potting.htm

Sorry, no data on hand for heat capacity, you would only need this in
addition to the thermal conductivity for a transient thermal analysis.

Kind regards,

Paul.
> ______________________ No Boundaries___________________
>                                           ANSYS, Inc.
> Paul Lethbridge
> Electronics Industry Specialist
>
>       email:  [email protected]
>       voice:  724.514.3124
>       fax:            724.514.3115
>       USPS:   275 Technology Drive, Canonsburg, PA 15317
>
> __________________ http://www.ansys.com _____________
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics
University Wafer